冬季泡沫混凝土保温板施工方法之调整配合比方法

发布时间:2017/3/24 18:01:56 浏览次数:454
本实用新型主要适用于0°C左右的泡沫混凝土保温板的施工。

冬季泡沫混凝土保温板施工方法之调整配合比方法

The utility model is mainly suitable for the construction of the foam concrete insulation board with a temperature of 0 DEG C or so.

具体做法:

Specific practices:

选择合适的水泥是提高混凝土抗冻性的重要手段。结果表明,应采用早强波特兰水泥。水泥的水化热较大,早期释放强度最高,3天抗压强度相当于普通波特兰水泥的抗压强度约为7天。



Selecting suitable cement is an important means to improve the frost resistance of concrete. The results show that early strength Portland cement should be used. The hydration heat of cement is larger, the early release intensity is the highest, and the compressive strength of 3 days is equivalent to the compressive strength of ordinary Portland cement for about 7 days.

尽量降低水灰比,略微增加水泥用量,从而增加水化热,缩短达到强度的时间。

As far as possible to reduce the water cement ratio, slightly increase the amount of cement, thereby increasing the hydration heat, shorten the time to achieve strength.

混合引气剂。在混凝土配合比不变的情况下,掺加引气剂产生的气泡,在水泥浆量相应增加,提高流动性的组合,提高其凝聚力和水水的压力使混凝土缓冲水冷冻保存,提高混凝土抗冻性。

Mixed air entraining agent. In the case of a constant ratio of concrete air entraining agent bubbles, a corresponding increase in the volume of cement slurry, improve liquidity, enhance the cohesive force and water pressure to the concrete buffer water freezing, improve the frost resistance of concrete.

加早强剂缩短混凝土凝结时间,提高混凝土早期强度。应用较常用的硫酸钠(掺量为2%的水泥)和MS - F复合早期强度的水试验剂(掺入水泥用量为5%)。

Adding early strength agent to shorten the setting time of concrete and improve the early strength of concrete. The application of the more commonly used sodium sulfate (2%) and the MS - F composite early strength water test agent (with a dosage of cement).

选择硬度高、间隙小的骨料,其热膨胀系数与周围砂浆相近。

The aggregate with high hardness and small clearance is selected, whose thermal expansion coefficient is similar to that of surrounding mortar.


合肥泡沫混凝土官方网站:http://www.ahzjcl.com/


最新内容:

上一篇: 冬季泡沫混凝土保温板施方法之蓄热法和抗冻外加剂
下一篇: 泡沫混凝土保温板冬季施工方法的选择
网站首页 | 公司简介 | 产品中心 | 工程案例 | 资讯动态 | 联系我们 | 在线咨询
安徽增杰建筑工程有限公司 版权所以
电话:13955134749     地址:安徽省合肥市庐阳区龙王路28号